Material Engineering / Adult Wellness OEM

Two silicone sex toys can carry the same Shore hardness specification yet feel noticeably different when pressed, bent or squeezed. The reason is simple: Shore hardness describes a material's response to a small indentation—not the complete product's stiffness.

Quick answer. Finished-product feel is a combination of silicone formulation, wall thickness, external dimensions, internal cavities, support structures and loading conditions. For an OEM brand, a hardness number is only the starting point. Geometry-controlled prototypes and functional tests are what confirm the intended feel.

This guide moves beyond the basics in our Shore hardness guide. It explains the engineering differences that matter when specifying a custom silicone product, approving samples and keeping repeat orders consistent.

1. Shore Hardness Is Not the Same as Product Stiffness

A Shore durometer presses a standardized indenter into a rubber sample and measures its resistance to penetration. Under ASTM D2240, the result depends on the selected scale, specimen preparation and test conditions. The method is useful for material identification and process control, but it is not a direct test of how far a complete toy bends.

For example, two molded parts might both be made from the same nominal 15 Shore A silicone. One is a slim flexible section; the other is a thick solid shape. The second can require much more force to bend even though the underlying material hardness is unchanged.

MATERIAL PROPERTY

Indentation hardness

How a standardized indenter presses into a tested silicone specimen under defined conditions.

Specify: Shore A or Shore 00, method, tolerance and conditioning.
FINISHED-PART RESPONSE

Flexibility and squeeze feel

How the whole product deforms under bending, compression or repeated handling.

Specify: load, displacement, location, temperature and acceptance range.

Important: Shore A and Shore 00 are different measurement scales. Do not compare unqualified numbers such as “20” across scales. Very soft materials may require Shore 00 or another suitable durometer type; the agreed test method matters as much as the number.

2. Why Wall Thickness Can Change the Feel So Much

Wall thickness is one of the most consequential design variables because bending is governed by both material properties and cross-sectional geometry. A thinner section is often easier to bend; a thicker one generally resists deformation, even when both use identical silicone.

Same silicone compound · same Shore hardness THINNER SECTION THICKER SECTION Greater deflection in this illustration Less deflection in this illustration Schematic only · not measured NEWTOP product test data
Figure 1. Identical silicone can respond differently because the section geometry changes. The drawing is conceptual, not a comparison of tested production samples.
Engineering insight

For an idealized rectangular beam in small-deflection bending, geometric stiffness depends on the cube of section thickness. Doubling thickness can increase the section's bending stiffness by roughly eight times if other variables remain constant. This is an illustrative mechanics relationship—not a prediction for complex, highly deformable silicone toys.

In practical development, engineers also inspect transitions between thick and thin areas. Abrupt changes can concentrate strain, complicate demolding or create weak points around narrow necks, ribs and undercuts. A smooth thickness transition may improve how the part bends and how it survives repeated handling.

3. Solid, Hollow and Layered Products Can Feel Different

External dimensions do not reveal the entire design. A solid silicone body, a hollow cavity and a soft outer layer over a firmer support may have very different force–deflection responses. Internal construction is therefore part of the product specification, not an optional detail.

Solid section Same compound throughout Hollow section Cavity changes deformation Layered section Soft skin + firmer core Conceptual cross sections · not to scale
Figure 2. Three ways to change finished-part response without relying on a single Shore number. Suitability depends on intended use, structural reliability and validated manufacturing methods.

Solid construction

Often gives more bulk resistance at a given overall geometry. Part weight, cooling, curing and internal uniformity all require review on large sections.

Hollow construction

A cavity can make an external shape more compliant or lighter. Wall stability, collapse, cleaning access and tear-prone transitions must be evaluated.

Dual-density construction

A softer outer zone paired with a firmer core can separate surface feel from structural support. Bonding, layer thickness and repeatable placement need verification.

Layered molding is not inherently better than single-material construction. It adds process and quality requirements. For an existing concept, start by establishing whether the desired performance can be achieved through simpler geometry changes before increasing process complexity.

4. Five More Variables Buyers Often Overlook

01

Overall length and leverage

Long, narrow sections bend more easily under a comparable end load than short, compact sections of the same cross-section. Where and how force is applied matters.

02

Local curves, ribs and transitions

Raised textures, neck diameters, junction radii and curvature change local resistance to deformation. The same product may feel firm in one area and flexible in another.

03

Surface finish and contact

Matte and glossy finishes, surface friction and contact area affect the perception of softness, even when measured bulk hardness remains similar. Surface feel and mechanical stiffness should be evaluated separately.

04

Different silicone formulations

Two compounds with similar durometer readings may differ in stress–strain response, rebound, tear strength or time-dependent recovery. A matching Shore number does not guarantee identical mechanical behavior.

05

Temperature and loading history

Silicone is viscoelastic. The force required to deform a part can depend on loading rate, time held under compression and temperature. Compare prototypes under the same conditions.

These variables help explain why switching to a new silicone grade is not always the fastest solution. Sometimes a targeted geometry change is more effective; sometimes a different compound is required. In either case, changes should be validated on molded samples.

5. What This Means for Different Adult Product Designs

Product requirements vary considerably. In an OEM review, we recommend defining the functional response needed in each zone instead of using a generic “soft” or “firm” instruction for the entire product.

Product featureWhat changes perceived feel?What to validate?
Solid molded bodySection diameter, overall length, shape transitionsDefined bend or compression force, dimensions
Thin flexible sleeveWall thickness, opening geometry, ribs and cavityStretch, recovery, tear resistance, shape retention
Soft-touch outer shellShell thickness, underlying support and surface finishLocal compression, assembly fit and finish consistency
Dual-density constructionOuter layer thickness and inner-core firmnessLayer position, bond integrity, bend response
Flexible base or neckUndercuts, flange thickness and junction radiiRepeated bending, tear initiation, functional stability

For a broader introduction to selecting a product range, see our size and firmness guide. For manufacturing options and private-label support, review our custom silicone adult toy manufacturing services.

6. How Should Brands Test “Feel” Before Mass Production?

There is no universal numerical test for consumer-perceived feel. A useful approval plan combines standardized material data with repeatable tests on the actual product. It is important to agree on the measurement location, loading direction and pass/fail criteria before comparing samples.

Material coupon Durometer test Finished product Force–deflection test Repeated loading Recovery and durability
Figure 3. A practical validation sequence. The exact fixtures, loads and acceptance criteria must be established for the product rather than inferred from these schematics.
CheckWhat it tells the buyerHow to make results comparable
Shore hardnessMaterial indentation resistanceState scale and method; use suitable specimens and conditioning.
Compression forceForce needed to squeeze a chosen product zoneFix probe/contact area, speed and compression distance.
Bend or deflection forceWhole-part flexibility under a defined loadFix the support span, loading point and displacement.
Recovery / repeated loadingWhether response changes after repeated deformationAgree number of cycles, dwell times and evaluation period.
Tensile and tear propertiesMaterial resistance to stretching and tear propagationUse consistent specimen and test conditions, such as suitable ASTM D412 and ASTM D624 methods.
Controlled sample reviewPerceived tactile quality and user feedbackUse agreed reference samples and recorded evaluation conditions.
A measurement trap: pressing a Shore durometer directly onto a curved or thin finished section can produce misleading readings if the method's specimen requirements are not met. For material approval, use appropriate test pieces prepared and tested under agreed conditions. A published study on silicone elastomers also documents thickness-related hardness measurement errors (research summary).

7. A Better OEM Approval Workflow: Material + Geometry + Sample

For private-label product development, the most reliable way to achieve consistent feel is to separate the three decisions that are frequently mixed together: which compound to use, how to design the geometry and how to approve finished samples.

01

Define the target experience

Identify which zone should compress, flex or maintain support, and what existing reference product or sample defines the target.

02

Select silicone grades

Confirm proposed Shore scale/range, relevant mechanical data, material traceability and target-market testing requirements.

03

Review geometry before tooling

Check thickness transitions, cavity dimensions, core placement, demolding and areas of concentrated stress.

04

Approve samples and test methods

Evaluate finished-part flexibility with consistent fixtures; document acceptable sample variation and visual criteria.

05

Control production batches

Keep the approved material grade, color, tooling, curing parameters and sample references aligned across repeat orders.

06

Revalidate design changes

If the wall thickness, core or compound changes, reassess functional feel rather than assuming the original Shore target guarantees equivalence.

At NEWTOP Silicone, OEM/ODM project discussions can cover design review, material hardness, tooling, molding and private-label packaging. Confirm the exact testing scope and measurable acceptance criteria in your project specification rather than relying on a generic “soft silicone” description.

8. What to Put in Your RFQ Instead of “Make It Shore A 10”

A useful RFQ communicates both material requirements and target product response. The following items make technical conversations more efficient:

  • Product drawing, dimensions and critical wall thicknesses
  • Solid, hollow or layered construction
  • Target Shore scale, hardness and tolerance
  • Reference sample or target tactile profile
  • Expected bending/compression test location
  • Repeatability and durability requirements
  • Appearance, surface finish and color
  • Target market, order quantity and packaging needs

For custom concepts or confidential development, share a sketch or CAD file and discuss feasibility before committing to new molds. See NEWTOP's silicone adult toy OEM/ODM capabilities for the product types and project services available.

Frequently Asked Questions

Can two silicone toys with the same Shore A hardness feel completely different?

Yes. Even if the measured material hardness is comparable, differences in thickness, length, cavities, structural support and surface characteristics can produce noticeably different deformation and tactile response.

Does a lower Shore hardness always mean a softer finished product?

Not necessarily. A thick part made from lower-hardness silicone can resist bending more than a thin part made from a higher-hardness compound. Compare the finished geometry under the same test conditions.

Is Shore hardness enough to specify silicone for mass production?

No. Include the durometer scale and method, material requirements, critical geometry, mechanical/durability tests and approved finished samples. Hardness alone does not establish strength or performance.

Should a brand change silicone hardness or wall thickness first?

It depends on the product. If material properties already meet the performance and safety requirements, geometry changes may be worth prototyping first. For other designs, a different grade or a layered construction may be necessary.

How can brands keep the same feel across repeat orders?

Keep an approved reference sample, a controlled material specification, consistent tooling and process settings, and finished-part test limits. Revalidate any meaningful changes to geometry or formulation.

Technical References

The engineering principles discussed here draw on ASTM D2240 (durometer hardness), ASTM D412 (tensile testing), ASTM D624 (tear strength) and published research on silicone specimen thickness and hardness measurements. Testing requirements should be selected for the specific product, application and applicable standards.